Hi guys,
Just a quick post to make sure I'm on the right path and ask for a little advice before I proceed further (and make another mess!
).
I've stripped back, cleaned and applied two coats of epoxy primer to the underside of my spitfire....
Both coats went on within an 18 hour window, both applied by brush. Next, later this evening I plan on seam sealing.
So, my questions:
1. I plan on using UPol Tiger Seal as a seam sealer, is this ok too use?
2. Over this I'll be applying Upol Gravitex Stonechip; I assume the best route is to dust a coat on, let it flash, then go on with a proper full coat?
3. Over the stonechip I plan on applying the cellulose base coat. What is the mixture ratio for the paint/thinner? Is the first light coat thinned more than the last coat?
Thanks for any help
Just a quick post to make sure I'm on the right path and ask for a little advice before I proceed further (and make another mess!

I've stripped back, cleaned and applied two coats of epoxy primer to the underside of my spitfire....

Both coats went on within an 18 hour window, both applied by brush. Next, later this evening I plan on seam sealing.
So, my questions:
1. I plan on using UPol Tiger Seal as a seam sealer, is this ok too use?
2. Over this I'll be applying Upol Gravitex Stonechip; I assume the best route is to dust a coat on, let it flash, then go on with a proper full coat?
3. Over the stonechip I plan on applying the cellulose base coat. What is the mixture ratio for the paint/thinner? Is the first light coat thinned more than the last coat?
Thanks for any help