I used to work on industrial oxidisers and dryers, we used to run them to temps up to about 1200 deg C. Stainless bolts after they had been through a heat cycle were a nightmare if they were fitted without any anti seize.
We used to use molykote products, there were a few types we used. Can’t recall the name but I’ve got a few tins kicking around the garage I’ll have a look later.