I have a SIP Migmate 150 turbo and very new to mig welding. Ive really only be practicing to date using disposable cyclinders with some good results (eventually)
I thought id upgrade to bottle gas, so bought a reg and bottle of argonshild light. I cant seem to get going on a weld without the wire fusing to the tip.
Any suggestions as to why this is happening. Im using some sheetmetal scraps maybe 3 mm, tried various wide settings .
any ideas ??
I thought id upgrade to bottle gas, so bought a reg and bottle of argonshild light. I cant seem to get going on a weld without the wire fusing to the tip.
Any suggestions as to why this is happening. Im using some sheetmetal scraps maybe 3 mm, tried various wide settings .
any ideas ??