There’s your problem. DPI can’t be done through paintThe welding was covered with primer paint before dye pt , it was cleaned but not properly that s why it looks like the dye was not removed entirely.

The welding itself was Grinded a Little to remove the paint, But not the base material ,There’s your problem. DPI can’t be done through paint![]()
@BDan21
The replies are all linked to the defect.
It will be hard to see and explain why, how or what the defect was. If the dye test is hiding, masking or not done correctly.