I run 2 Fronius tps 500i attached to Kuka Robotic arms and I'm struggling with heat zones on my spike welds, they're 40mm long welds on 32x40x50 spike being welded to a long plate 90x800x30, the settings are Steel M21 Ar + 15-20% C02 with 1.2mm wire and the welder settings are 273amps 26.4v and 8.7m/min wire feed.
The weld looks good but the heat dispersal is too high and not enough penetration causing the spike to come off after a few hits of a hammer.
any help would be appreciated.