I have been soaking my cold rolled steel in a citric acid bath for a day then cleaning off the scale with a paint removal disk.
If box section, I have squirted a hose pipe through the middle to wash out the acid then pulled a cloth through to dry it and clean it out a bit.
Is this enough, or should I be doing more to neutralise the acid?
If box section, I have squirted a hose pipe through the middle to wash out the acid then pulled a cloth through to dry it and clean it out a bit.
Is this enough, or should I be doing more to neutralise the acid?