Hi fellas, been off for some time...well, I got myself a Telwin Tecnica 155 (150 amps). It has HF, and pre/post flow settings for argon...I am quite happy with it "cos I got it purely for when I need neater weld than MIG or OXY/ACET.
However I have been trying to weld thin steel/stainless sheet( 0.8mm), and blew holes even with 25amps,when I get it down to 15amps, it will take age to melt the metal
Do you think that this is possible WITHOUT filler rod?
Regarding aluminium, can it be welded even though it will not be so neat?(it's only DC)...any techniques/tips?