Just finished straighting up my garage and built my "welding bay" today. I have just done my first practice welds with my new Clarke 135TE.
I used a piece of new, clean 1mm thick steel. All the welds were done on setting 1-min (lowest) and I tried several wire speeds but 5 seemed the best. I'm using argonshield light gas.
Pictures:
Reverse:
A few questions:
What is the brown stuff you can see on the front of the metal, is that normal or am I doing something wrong.
Also the window in my mask (Sif lite auto darkening) has a tendency to fog up, any way of stopping it?
Thanks.