Robert1998
Forum Supporter
- Messages
- 225
- Location
- Spain
Grettings from Sevilla, a very dry place in Spain. But not this autum.
It is raining a lot and my shop isn´t very isolated. The air has a lot of humidity and everithing is rusting. I usually use WD40 but it seems not enought, or maybe I haven´t put egnough quantity. Any advice?
After cleaning the table of the mill, I have use steel wool (is that proper?) some stains remain. Should I insist to try to eliminate them or only need to keep the table clean and lubricated?
And other question, the chips (dust) from cast iron, Is it very abrassive? A little get in the ways of the lathe and I don´t know if it is really important to disassmebly the carriage to clean it.
Thank you
It is raining a lot and my shop isn´t very isolated. The air has a lot of humidity and everithing is rusting. I usually use WD40 but it seems not enought, or maybe I haven´t put egnough quantity. Any advice?
After cleaning the table of the mill, I have use steel wool (is that proper?) some stains remain. Should I insist to try to eliminate them or only need to keep the table clean and lubricated?
And other question, the chips (dust) from cast iron, Is it very abrassive? A little get in the ways of the lathe and I don´t know if it is really important to disassmebly the carriage to clean it.
Thank you