As @Misterg says, 5% CO2 in Argon will be best for anything upto about 6 or 7 mm. Thicker than that you'll be better with 15% CO2 (and possibly a bigger welder! ) Not sure about Adams but Hobby Weld add 2% O2 which apparently makes for less splatter.