Hi, I'd just like some thoughts on this weld of mine. My settings were 80 (about 27 to 30V) and 6.0 (about 250A). Gas was an Argon mix, at 20l/min. I executed a slight weave. I tried to nudge just at the leading edge of the puddle, watching the toes of the weld to maintain an even fill. What can I improve here? There was some patter, everything you see is uncleaned. About a 45 degree work angle and maybe 15 degree travel angle. I think the tie ins at the end of the weld could be better, and perhaps the start of the weld. Maybe hold it more, or back into it after start for better fusion? Am I over thinking it? I'm using 1.2mm wire. Any advice much appreciated.