Used one by Permabond to stick 3 bits of 12mm steel plate together before milling and linishing. Incredibly strong.
I was concerned the heat from the linisher would break the bond.
No chance! It took 15 mins with a blow lamp to heat it enough. I had an infrared thermometer. Needed 220c before it let go!
So many uses!
I was concerned the heat from the linisher would break the bond.
No chance! It took 15 mins with a blow lamp to heat it enough. I had an infrared thermometer. Needed 220c before it let go!
So many uses!