Shox Dr Chief Engineer to Carlos Fandango Messages 17,986 Location East Yorkshire Nov 10, 2008 #2 I weld a lot of 0.9mm Zinctec. Tight outside corner 28amps. Lap 36amps. both either fused or with rod
I weld a lot of 0.9mm Zinctec. Tight outside corner 28amps. Lap 36amps. both either fused or with rod