Hasbean try and get hold of some esab mildtrodes if you can, i know it will be difficult from your end of the world, but on my IFL 200phf (same as yours just has fancy TIG circuitry) when welded and the slag is chipped it looks like the weld has been polished with rubbing compound, real nice weld with excellent penetration.