Hi, Im using a BOSS (Weldmate) P170P with flux cored wire (gasless). I often change between gas and gasless depending on location and material.
Lately I'm repeatedly getting porous welds with my gasless wire on std mild steel.
I Have triple-checked all the obvious things (polarity, wire, tip, etc) but still cant figure out if its me or the welder ?
Any help would be much appreciated.
Thanks, Matt
Lately I'm repeatedly getting porous welds with my gasless wire on std mild steel.
I Have triple-checked all the obvious things (polarity, wire, tip, etc) but still cant figure out if its me or the welder ?
Any help would be much appreciated.
Thanks, Matt