I have to skin some frames that have been fabricated from 60 X 40 x 2.5 RHS with 0.9mm sheet.
The box section frames are approx 2.1 metres wide x 1.8m high . The 40 wide bit is what we are attaching to.
Welding will cause too much distortion, so bonding is going to be best option. The finish needs to be smooth ( otherwise I would have probably riveted them).
What would you recommend. Not looking for a cheap product , nor mega expensive. Just want something that is not going to let go when cured.
There are 20 of the big ones 7 of the small window and 3 of the other ones to do, so its going to require quite a bit.
I have to skin some frames that have been fabricated from 60 X 40 x 2.5 RHS with 0.9mm sheet.
The box section frames are approx 2.1 metres wide x 1.8m high . The 40 wide bit is what we are attaching to.
Welding will cause too much distortion, so bonding is going to be best option. The finish needs to be smooth ( otherwise I would have probably riveted them).
What would you recommend. Not looking for a cheap product , nor mega expensive. Just want something that is not going to let go when cured.
There are 20 of the big ones 7 of the small window and 3 of the other ones to do, so its going to require quite a bit.