So i need some assistance please, Below is my first attempt at Tig Ally welding and not a pretty sight.
1.6mm filler
Grey tungsten pointed but not sharp about 8mm from end of shroud
50A
Post set to 8.0
Suggestions as to what direction to get improved results, And no I'm not selling it yet !
1.6mm filler
Grey tungsten pointed but not sharp about 8mm from end of shroud
50A
Post set to 8.0
Suggestions as to what direction to get improved results, And no I'm not selling it yet !