Hi all, looking for help please
Just carried out some repairs to on my old car bodywork, filled, smoothed, primed and painted. Taking a lot of time getting things smoothed out it seems Iv'e wasted a long time as after spraying cellulose paint 50/50 mix on top the repair the filler has sunk or shrunk and there is a ring around the repair. I used a upol product for the filler.Where I was expecting a light polish and "job done"it looks a mess.
Any ideas what causes this and how to overcome it please. As Iv'e still lots to topcoat, I wonder if " bar coat "will help applied over the panels Iv'e allready prepped and yet to be topcoated .???
Thanks
Just carried out some repairs to on my old car bodywork, filled, smoothed, primed and painted. Taking a lot of time getting things smoothed out it seems Iv'e wasted a long time as after spraying cellulose paint 50/50 mix on top the repair the filler has sunk or shrunk and there is a ring around the repair. I used a upol product for the filler.Where I was expecting a light polish and "job done"it looks a mess.
Any ideas what causes this and how to overcome it please. As Iv'e still lots to topcoat, I wonder if " bar coat "will help applied over the panels Iv'e allready prepped and yet to be topcoated .???
Thanks