Hello there
I have welded aluminum with my 1/16 tungsten although the arc doesnt show focused i get a nice weld pool.
But recently i went with a larger tungsten electrode 3/32 for more amperes, but the arc is not visible and it look like it goes here and there.
What are some tricks to minimize that ?
I have set my frequency setting to maximum, should i make a pointed end ?
Protrusion of the tungsten ? Any other tips ?
I have welded aluminum with my 1/16 tungsten although the arc doesnt show focused i get a nice weld pool.
But recently i went with a larger tungsten electrode 3/32 for more amperes, but the arc is not visible and it look like it goes here and there.
What are some tricks to minimize that ?
I have set my frequency setting to maximum, should i make a pointed end ?
Protrusion of the tungsten ? Any other tips ?