Noods
Member
- Messages
- 979
- Location
- Ipswich
Tried a little pulse today for the very first time with my new welder..
Plenty to learn still obv and as always very willing..
Set up..
DC tig with pure argon.. 1.6mm stainless steel sheet, outer angle joint, no filler, gas lense, 1.6mm electrode, red tip,
Peak set 130amps
Lower value 30% of peak
Pulse @1.5
Background 5% pulse
Used a pair of 6mm thick steel stock ( clean) as chill bars. Would like copper but no luck finding yet..
Happy for any advice to improve ..
Picture is as it came out no cleaning at all..
Plenty to learn still obv and as always very willing..
Set up..
DC tig with pure argon.. 1.6mm stainless steel sheet, outer angle joint, no filler, gas lense, 1.6mm electrode, red tip,
Peak set 130amps
Lower value 30% of peak
Pulse @1.5
Background 5% pulse
Used a pair of 6mm thick steel stock ( clean) as chill bars. Would like copper but no luck finding yet..
Happy for any advice to improve ..
Picture is as it came out no cleaning at all..