Hi averyone, we braze blades with heneycomb, both from nickel alloys, the problem is, after vacuum furnace we have braze metal droplets on airfoil. We dry the brazing paste before furnace loading minimum 3 hours. Maybe someone can give some tips. Many thanks.
Apologies Grossinka.
I know nothing about this one. Somebody here must know what you are talking about. It sounds interesting.
Can you explain what you are doing to a brainless artist.?
Believe me there are people on this website who do understand this stuff.
Try copying this thread into the tools materials and techniques section.
In fact I am telling you to repost. So There.
Chunko'.
Edit, where did that come from??