Cris B
Every day welding is a school day
- Messages
- 503
- Location
- Sefton
I need to be able to form up some 5mm aluminium bar probably 50mm wide by putting some 90 degree bends into it. Aluminium is EN AW 6060.
What is the best way to form these bends. I have a sheet metal folder that copes with SWG16 in good widths - will this be up to the job?
Is cold forming okay or is heat needed?
What the best way to protect the anodised finish? Masking tape?
What is the best way to form these bends. I have a sheet metal folder that copes with SWG16 in good widths - will this be up to the job?
Is cold forming okay or is heat needed?
What the best way to protect the anodised finish? Masking tape?