A little frustrated.. overall been welding really well with my little 160 amp Tig.. however, still getting a real problem with holes but only at the start and end of a run.. been butt welding 2.5mm ss with red 1.6mm electrode no7 ceramic 1.6mm ER rod at 40amps slope set at 2 pure argon gas set at 10.. have leak tested and none found!
Any ideas please..